Performance Testing of Flexible Cementitious

General Product Description

Flexible cementitious is generally a 2-part, polymer-modified cementitious waterproofing system.

Critical Conditions to Note

Weather conditions such as ambient temperature, precipitation, and humidity can affect the quality of the application and performanceof the product. Cementitious membrane systems require a damp surface to improve the adhesion of membrane to the concrete surface. However, standing water must be removed from the concrete surface. The concrete surface should be saturated with clean water to achieve saturated surface-dry (SSD) condition prior to the application of the first coat of waterproofing membrane. Concrete surface that is under constant immersion or with an active hydrostatic head of water may not be suitable for usage of flexible cementitious. Flexible cementitious waterproofing membrane is not suitable to be used as an exposed system.

Recommendations for Laboratory Testing Conditions

Type of Tests Recommended Curing Conditions
Tensile Strength and Elongation Consistent 23°C and 70% relative humidity for a period of 28 days
Adhesion to Concrete 23°C and 50% relative humidity for a period of 28 days

 

Type of Tests  Recommended Testing Conditions
Tensile Strength and Elongation Testing conditions: 23°C and 50% relative humidity. Specimens shall be conditioned for at least 3 hrs when the test temperature is 23°C. Maintain relative humidity at 50 ± 5% and condition the specimens for at least 24 hours prior to testing.
Adhesion to Concrete

 

Type of Tests Recommended Curing/Testing Conditions for Quick test
Tensile Strength and Elongation 1. Curing condition at 70% relative humidity for 7 days.
2. Testing conditions with specimens conditioned at 40°C for 30 mins without air cycling. Maintain relative humidity at 50% and condition the specimens for at least 30 mins prior to testing.

 

Type of Tests Recommended Testing Equipment Loadcell and Speed
Tensile Strength and Elongation 500mm / min with dumb-bell Die C Specimen using up to a maximum load cell capacity of 100N.

 

Type of Tests Recommended Testing Conditions
Adhesion to Concrete At least 28-day cured concrete is used as the substrate for application of waterproofing membrane for test

 

gcpat.id | For technical information: asia.enq@gcpat.com

We hope the information here will be helpful. It is based on data and knowledge considered to be true and accurate, and is offered for consideration, investigation and verification by the user, but we do not warrant the results to be obtained. Please read all statements, recommendations, and suggestions in conjunction with our conditions of sale, which apply to all goods supplied by us. No statement, recommendation, or suggestion is intended for any use that would infringe any patent, copyright, or other third party right. 

© Copyright 2021 GCP Applied Technologies, Inc. All rights reserved.
 


GCP Applied Technologies Inc., 2325 Lakeview Parkway, Alpharetta, GA 30009, USA
PT GCP Applied Technologies Indonesia, Cikarang Industrial Estate Kav C-32, Cikarang, Bekasi 17530
This document is only current as of the last updated date stated below and is valid only for use in Indonesia. It is important that you always refer to the currently available information at the URL below to provide the most current product information at the time of use. Additional literature such as Contractor Manuals, Technical Bulletins, Detail Drawings and detailing recommendations and other relevant documents are also available on www.gcpat.id. Information found on other websites must not be relied upon, as they may not be up-to-date or applicable to the conditions in your location and we do not accept any responsibility for their content. If there are any conflicts or if you need more information, please contact GCP Customer Service.